Technical Guide

What Is Sector Welding? The Advanced Bore Repair Technique Explained

Sector welding deposits weld only on the worn face of asymmetric bores — reducing wire consumption, heat input, and repair time. Available exclusively on the BOS DS60.

Prakhar Bhardwaj · Founder — BOS · In collaboration with ENZO Digital Editorial Team · August 2026 · ~12 min read
DS60 Only
Machine Required
65–600 mm
Bore Range
90°–180°
Typical Weld Arc
~60% Less
Weld Wire Used
H7 ±0.05 mm
Final Tolerance

1. Introduction

Most bore wear is not uniform. If you look at a worn excavator bucket pin bore under a bore gauge, you will rarely find a bore that has worn evenly around the full circumference. What you find instead is a bore that has worn more on one side than the other — the side that carries the working load.

For decades, the standard approach to bore welding did not distinguish between uniform and asymmetric wear. Weld was deposited around the entire bore circumference regardless of where the wear was actually concentrated. This worked — but it was wasteful. Excess weld material on the unworn side of the bore meant excess heat input, excess post-weld boring time, and excess material cost. On high-alloy components like crane boom pins and mining equipment joints, that excess heat also meant distortion risk.

Sector welding was developed to address exactly this problem. It is the advanced bore welding mode that deposits weld material only on the specific arc — the "sector" — of the bore where wear has actually occurred. No weld on the unworn side. No excess heat. No excess material. Faster repair. Better result.

This guide explains what sector welding is, how it works, when you need it, and why it is available exclusively on the BOS DS60 — not the DS50.


2. Understanding Asymmetric Bore Wear

To understand sector welding, you first need to understand why bore wear is asymmetric.

A pin-and-bore joint carries load in a specific direction determined by the machine's operating cycle. An excavator bucket pin bore is loaded predominantly downward during the digging cycle — the bucket pulls against the earth, and the load passes through the pin in a consistent direction. A crane boom pin is loaded in the direction of the lifted load. A jaw crusher toggle bore is loaded in the direction of the crushing force.

This directional loading means that one face of the bore — the "loaded face" in the direction of the working force — contacts the pin with significantly greater pressure than the opposite "relief face." Over time, the loaded face wears faster. The bore becomes oval, not because the pin is spinning randomly, but because it is pressing consistently against one side.

"The bore becomes oval not because the pin is spinning randomly, but because it is pressing consistently against one side. Sector welding treats this localised problem with a localised solution."

The result is a bore that looks like this in cross-section: worn significantly on one arc of perhaps 90 to 180 degrees, and still close to original specification on the remaining arc. Depositing weld around the full 360 degrees of this bore treats a localised problem with a global solution. Sector welding treats it precisely where it is needed.


3. What Is Sector Welding?

Sector welding is a programmable bore welding mode in which the welding head deposits material only on a defined arc — or "sector" — of the bore circumference. The operator programs the start angle, the end angle, and the arc length of the weld deposit on the DS60's numerical control panel. The welding head then executes this programmed arc exactly, stopping and pausing at the programmed boundaries rather than continuing around the full circumference.

The result is a bore where fresh weld material exists precisely where wear occurred, and the original bore surface is preserved where it was still within tolerance. When the boring phase follows, the boring head machines the entire bore circumference — removing only the excess from the weld deposit on the worn arc, and taking only a finishing cut from the unworn arc to restore overall roundness and surface finish.

Key Operational Parameters

  • → Start angle — The angular position at which weld deposition begins, measured from a reference point on the bore. Set based on bore measurement.
  • → End angle — The angular position at which weld deposition ends. The difference between start and end angle defines the weld arc length.
  • → Arc length (sector size) — The total arc to be welded, typically 90 to 180 degrees. Cranes: 90–120°. Crushers: 150–180°.
  • → Feed rate — How fast the welding head advances along the bore axis per revolution — applied only within the programmed arc.
  • → Welding speed (rotation) — Slightly slower than inner circle welding to ensure proper fusion on weld boundaries.
  • → Passes — Number of weld passes to build the bore back to target diameter. Multiple passes on the loaded face before a final pass brings the full sector to uniform height.

4. The Three BOS Welding Modes Compared

The BOS DS60 supports three welding modes. Understanding the difference is essential for selecting the right approach. For a full comparison of the two machines, see our DS50 vs DS60 comparison.

Welding Mode What It Does Wear Pattern Addressed Machine
Inner Circle Welding Deposits weld continuously around the full 360° bore circumference Uniform wear — bore worn evenly all around DS50 and DS60
Sector Welding Deposits weld on a programmed arc only — e.g., 120° on the worn face. Stops at arc boundaries. Asymmetric wear — one-sided loading damage. Crane, crusher, mining bores. DS60 only
Jump Welding Deposits weld in defined segments, skipping programmed intervals around the circumference Partial wear — some sections still within tolerance. Also avoids grease holes and ports. DS60 only

Table 1 — BOS Welding Modes: Inner Circle vs Sector vs Jump. The DS50 supports inner circle welding only — correct for the majority of standard construction equipment bore repairs.


5. When Is Sector Welding the Right Choice?

Sector welding is the correct approach when bore measurement confirms that wear is concentrated on one arc of the bore rather than distributed uniformly around the circumference.

Equipment / Application Why Sector Welding Typical Weld Arc
Crane boom pins Cranes lift in a consistent direction — boom pin loads on one face every time. Classic one-sided asymmetric wear. 90–140°
Mining excavator bucket bores High-cycle abrasive loading in consistent digging direction. Wear concentrated on leading face. 90–150°
Jaw crusher toggle bores High one-directional crushing force. Toggle bore loads asymmetrically every cycle. 120–180°
Rope shovel dipper pivot bores Consistent one-direction working force produces heavy asymmetric wear on loaded face. 120–180°
Dump truck body hinge bores Body lifts in one direction — hinge bore loads on the lift side. Asymmetric wear typical. 90–120°
Marine rudder pintle bores Tidal and steering forces create directional loading. Asymmetric wear on current-facing bore surface. 90–150°
Articulated vehicle pivot bores Steering and working loads create consistent directional force on pivot bore. 100–150°

Table 2 — Applications where sector welding is recommended over standard inner circle welding.

Diagnostic Test

Take bore gauge measurements at 45-degree intervals around the bore circumference. If readings show more than 1.5 mm variation between maximum and minimum, the wear is asymmetric and sector welding is the better choice. If measurements are within 1 mm of each other, standard inner circle welding is sufficient.


6. Benefits of Sector Welding Over Inner Circle Welding for Asymmetric Bores

Less Weld Material — Lower Cost

Depositing weld on 120° instead of 360° uses approximately one-third of the welding wire. For large bore diameters in mining and crane applications, sector welding reduces material cost by ₹400–₹2,000 per repair.

Less Heat Input — Reduced Distortion

A 120° sector weld introduces approximately one-third the heat of a full-circle weld. For crane structural steel, mining equipment Hardox bores, and marine stainless components, this meaningfully reduces distortion risk.

Less Post-Weld Boring Time

The boring head takes a full-depth cut only through the weld arc and a light finishing cut over the unworn arc. A 120° sector weld reduces boring material removal by approximately 67% compared to full-circle.

More Precise Repair Geometry

The repaired surface on the loaded face is fresh weld deposit — typically harder and more wear-resistant than the original parent material. The repair geometry matches the actual wear mechanism of the joint.

Reduced Operator Dependency

On the DS60, sector welding parameters are programmed numerically — start angle, end angle, arc length, feed rate. The machine executes these parameters consistently regardless of which operator is running it. For fleet maintenance operations with multiple technicians, numerical sector welding produces the same quality from every operator.


7. Sector Welding vs Jump Welding — What Is the Difference?

Both sector welding and jump welding are advanced modes available exclusively on the BOS DS60. Both address wear patterns that inner circle welding handles suboptimally. But they address different wear patterns.

Sector welding addresses asymmetric wear — a bore that has worn more on one continuous arc (the loaded face) than the rest.

Jump welding addresses interrupted wear — a bore that has worn at multiple separated points around the circumference, with areas between the worn zones still within tolerance. Jump welding also skips grease holes, ports, and fittings that cannot receive weld material.

Comparison Point Sector Welding Jump Welding
Wear pattern One continuous worn arc (loaded face) Multiple separated worn zones around circumference
Programming Start angle + end angle (one continuous arc) Multiple arc segments with skip intervals
Typical use Crane pins, crushers, rope shovels Partially worn excavator bores, bores with grease holes
Heat input vs inner circle Lower — proportional to sector size Lower — proportional to welded arcs vs total circumference
When to choose Bore gauge shows one face significantly more worn Bore gauge shows multiple worn zones with good areas between

Table 3 — Sector Welding vs Jump Welding. In some repairs, both modes are combined — e.g., sector welding for the main loaded arc with jump welding to skip a grease hole.


8. Why Sector Welding Requires the BOS DS60

Sector welding requires numerical control to execute correctly. The welding head must start depositing weld at a precise angular position, continue through a defined arc, and stop at a precise end point — then advance along the bar and repeat the same arc on the next pass. This requires the machine to know and control its angular position continuously throughout the weld cycle.

The BOS DS50 uses manual and automatic control modes where the operator sets parameters but does not program specific angular positions for weld start and stop. This is entirely adequate for inner circle welding where the weld runs continuously around the bore. It cannot support sector welding because there is no mechanism for the machine to hold and execute specific angular programming.

The BOS DS60's numerical control panel allows the operator to input start angle, end angle, feed rate, rotation speed, and number of passes as specific numbers. The DS60 then executes these parameters mechanically, maintaining angular position control through the gearbox and servo drive system. This is the technical basis for sector welding capability.

"For operators whose work includes crane pins, mining equipment, crushers, or any equipment with asymmetric bore wear patterns, the DS60's sector welding capability is not a luxury feature — it is the reason the machine exists."

For a detailed comparison of which machine fits your work, see the DS50 vs DS60 comparison guide.


9. Case Study — Sector Welding on Crane Boom Pins, North India

A crane service contractor based in North India was managing maintenance for a fleet of 8 mobile cranes used in infrastructure construction. The crane boom pins were requiring bore repair every 4–5 months — significantly more frequently than the expected 8–10 month interval.

Bore measurements taken before repair showed consistently asymmetric wear: the boom pivot bore was worn 3–4 mm deeper on the load face than on the relief face. The crane lifts predominantly in one direction on a typical infrastructure site — toward the working area — creating predictable one-sided loading on the boom pin bore.

Prior repairs had used inner circle welding — depositing a full circumference of weld regardless of the wear pattern. This was technically sound but inefficient: the relief face received weld it did not need, introducing unnecessary heat into the crane boom structure.

After Switching to Sector Welding on BOS DS60

Weld Wire Consumption
↓ ~60%

110° sector vs full 360° circle

Post-Weld Boring Time
↓ ~45%

Less material to remove after welding

Total Repair Time Per Bore
~3 hrs

Down from ~5 hrs with inner circle welding

Re-Repair Interval
7–8 months

Up from 4–5 months with inner circle welding

The sector welded bore surface on the load face is harder and more wear-resistant than the original parent material — fresh weld deposit versus original steel that had already been fatigued by years of cyclic loading. The repair itself performs better than the original bore.

Identifiable details withheld at client's request. Results reflect specific operating conditions.


10. Frequently Asked Questions

Sector welding is an advanced bore welding mode that deposits weld material only on a defined arc — or "sector" — of the bore circumference rather than the full 360 degrees. It is used when bore wear is asymmetric — concentrated on one face of the bore due to directional loading. Sector welding deposits material precisely where wear occurred, reducing weld wire consumption, heat input, and post-weld boring time compared to full inner circle welding.
Use sector welding when bore gauge measurements show that wear is asymmetric — when one face of the bore is worn significantly more than the other. If measurements taken at 45-degree intervals around the bore show more than 1.5 mm variation between maximum and minimum readings, sector welding is the more efficient and technically correct choice. Typical applications: crane boom pins, jaw crusher toggle bores, mining excavator bores, and rope shovel dipper pivots.
Sector welding requires numerical control capability. On the BOS range, sector welding is available exclusively on the BOS DS60, which has a digital numerical control panel for programming start angle, end angle, arc length, feed rate, and rotation speed. The BOS DS50 supports inner circle welding only and cannot perform sector welding.
For a typical crane boom pin bore with 120° asymmetric wear, sector welding reduces weld wire consumption by approximately 60–65% compared to full inner circle welding. Post-weld boring time reduces by approximately 40–50%. Total repair time reduces by 25–35%. Material cost saving per bore is typically ₹500–₹2,500 depending on bore diameter and wire grade. Time saving per bore is typically 1–2 hours.
Neither stronger nor weaker — correctly performed sector welding produces the same repair quality as inner circle welding on the areas where weld is deposited. The load-carrying surface of the bore receives a fresh weld deposit that is typically harder and more wear-resistant than the original parent material. The unworn face retains original material with only a finishing cut. Total joint strength is unchanged.
Sector welding addresses wear on one continuous arc — the loaded face. Jump welding addresses wear at multiple separated points around the bore circumference, with unworn areas between them. Sector welding programs one continuous start-to-end arc. Jump welding programs multiple separate weld segments with skip intervals. Both are available on the BOS DS60 only.
Yes — sector welding works across all bore diameters within the BOS DS60's range (65–600 mm). The programming parameters scale with bore diameter and arc length. Larger bores require proportionally more weld passes, but the mode functions the same regardless of bore size.
Measure the bore diameter at 45-degree intervals around the circumference. The worn arc corresponds to the angular range where measurements exceed the target specification. Add 10–15 degrees on each side as a buffer for the wear transition zone. For most crane and mining bore repairs, this produces a sector of 90–180 degrees.

11. References

1. PR Crane & Earthmovers / BOS — DS60 product documentation and field service records.

2. BOS — Bore On Site: Sector welding case study data, 2022–2026.

3. ISO 286-1 — Geometrical Product Specifications: Limits and fits (H7 tolerance system).

4. Caterpillar Inc. — Excavator and crane pin joint service specifications.

5. Komatsu — Equipment maintenance standards for boom and arm pin clearance tolerances.

6. FieldFix — Heavy Equipment Line Boring Repair Guide (fieldfix.ai, 2026).

Need Sector Welding for Your Bore Repair?

The BOS DS60 is the only portable line boring machine with sector welding, jump welding, and inner circle welding — all in one unit. Available for on-site deployment across India.

Prakhar Bhardwaj — Founder, BOS
Prakhar Bhardwaj
Founder — BOS

Prakhar Bhardwaj is the founder of BOS — Bore On Site, India's specialist portable line boring service. He writes BOS's technical guides on advanced bore repair techniques including sector welding, jump welding, and line boring for heavy equipment across construction, mining, and marine applications.

wearebos.in